Citation: | Liu Xiao, Wang Hui, Xiao Jun, Sun Yongduo, Liu Shuaiyang, Zhang Jinyu. Effect of Thermal Aging on Mechanical Properties of Silicon-containing Ferritic/Martensitic Steel[J]. Nuclear Power Engineering, 2023, 44(S1): 147-151. doi: 10.13832/j.jnpe.2023.S1.0147 |
[1] |
李辉,李烁,史春丽,等. 超低碳低活化铁素体/马氏体钢的低温韧性[J]. 金属热处理,2018, 43(1): 22-27. doi: 10.13251/j.issn.0254-6051.2018.01.005
|
[2] |
ALLEN T R, KAOUMI D, WHARRY J P, et al. Characterization of microstructure and property evolution in advanced cladding and duct: materials exposed to high dose and elevated temperature[J]. Journal of Materials Research, 2015, 30(9): 1246-1274. doi: 10.1557/jmr.2015.99
|
[3] |
KLUEH R L. Ferritic/martensitic steels for advanced nuclear reactors[J]. Transactions of the Indian Institute of Metals, 2009, 62(2): 81-87. doi: 10.1007/s12666-009-0011-3
|
[4] |
ZHANG J S. A review of steel corrosion by liquid lead and lead–bismuth[J]. Corrosion Science, 2009, 51(6): 1207-1227. doi: 10.1016/j.corsci.2009.03.013
|
[5] |
ZHANG J S, LI N. Review of the studies on fundamental issues in LBE corrosion[J]. Journal of Nuclear Materials, 2008, 373(1-3): 351-377. doi: 10.1016/j.jnucmat.2007.06.019
|
[6] |
SCHROER C, TSISAR V, DURAND A, et al. Corrosion in iron and steel T91 caused by flowing lead-bismuth eutectic at 400℃ and 10-7 mass% dissolved oxygen[J]. Journal of Nuclear Engineering and Radiation Science, 2019, 5(1): 011006. doi: 10.1115/1.4040937
|
[7] |
WEISENBURGER A, SCHROER C, JIANU A, et al. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models[J]. Journal of Nuclear Materials, 2011, 415(3): 260-269. doi: 10.1016/j.jnucmat.2011.04.028
|
[8] |
丁君艳. 9-12%Cr铁素体/马氏体耐热钢的显微组织和力学性能研究[D]. 淄博: 山东理工大学, 2008: 39.
|
[9] |
宋亮亮. 含硅9Cr-ODS钢设计与性能研究[D]. 合肥: 中国科学技术大学, 2018: 62-65.
|
[10] |
CHEN S H, RONG L J. Effect of silicon on the microstructure and mechanical properties of reduced activation ferritic/martensitic steel[J]. Journal of Nuclear Materials, 2015, 459: 13-19. doi: 10.1016/j.jnucmat.2015.01.004
|
[11] |
SAINI N, MULIK R S, MAHAPATRA M M. Study on the effect of ageing on laves phase evolution and their effect on mechanical properties of P92 steel[J]. Materials Science and Engineering:A, 2018, 716: 179-188. doi: 10.1016/j.msea.2018.01.035
|
[12] |
BYUN T S, HOELZER D T, KIM J H, et al. A comparative assessment of the fracture toughness behavior of ferritic-martensitic steels and nanostructured ferritic alloys[J]. Journal of Nuclear Materials, 2017, 484: 157-167. doi: 10.1016/j.jnucmat.2016.12.004
|
[13] |
ZHAO Y Y, LIANG M T, ZHANG Z Y, et al. Fracture toughness and fracture behavior of CLAM steel in the temperature range of 450℃-550℃[J]. Journal of Nuclear Materials, 2018, 501: 200-207. doi: 10.1016/j.jnucmat.2018.01.039
|